  • Jcope
    replied to New member
    This was done tonight.
    Voltage. D
    .035 wire
    tip distance about 3/4”
    See more | Go to post

    Leave a comment:


  • Jcope
    replied to New member
    Thanks for the responses.
    i am using .035 flux wire. MYweld brand
    I am welding soft steel square tube 1/16” wall thickness
    i have tried various voltage settings and have settled on D
    wire speed is near setting #2 on the Lincoln.
    Volt polarity is at (-)
    ...
    See more | Go to post

    Leave a comment:


  • Jcope
    started a topic New member

    New member

    Hello. Just joined up. I’m an old guy not willing to give it up. I live in Jackson, TN. USA.
    im currently involved in the construction of a sort of utility Kart to use around the place. It is an electric motor driven and a metal frame. I own a Lincoln 100 Welpak I’ve had for around 30 years...
    See more | Go to post
    Last edited by Jcope; 09-16-2023, 09:02 PM.