Hello bson, I just thought I'd lyk that i just experienced the exact same thing. I tried everything from brushing/acetone, different thicknesses, preheating, both ER5356 n ER4043, changing Argon pressure, new wire, I even moved the welder to an AWG 8 circuit.....the weld pool simply would not penetrate....