  • abunaitoo
    replied to Mig liner
    No problems at all.
    No kinks.
    Feeds well.
    I guess I'll just leave it alone.
    Thanks
    See more | Go to post

    Leave a comment:


  • abunaitoo
    started a topic Mig liner

    Mig liner

    Have an old Hobart 140.
    I've never changed the liner for the hose.
    Is there a reason why it needs to be changed????
    What problem would I have if it's bad?????...
    See more | Go to post

  • abunaitoo
    replied to Gas regulator
    The AF150 is suppose to be for Co2.
    Had to get an adapter for it.
    Same as with the tube one.
    Had to get an adapter.
    Never had a problem with the regulator freezing.
    I wonder if I'm pushing to much Co2 through the tube flowmeter???
    I setting it by the graduations...
    See more | Go to post

    Leave a comment:


  • abunaitoo
    started a topic Gas regulator

    Gas regulator

    First post here.
    Hope to learn more about this welder.
    Hobart 140. Got it around 1989.
    Light welding, Just for home hobby use.
    Use Co2 gas now, but used to use mix.
    Just to expensive these days.
    I have been using a Victor AF150.
    The diaphragm leaked, so I tried...