  • Buckman86
    replied to The blob!
    Bingo!
    its aluminum wire. I have a bad case of selective reading. I read mig and 0.035 when I bought the wire and must have over looked down to the right where it says aluminum. I had to tear off the label to put it so I couldn’t read it after the fact.
    many thanks everyone....
    See more | Go to post

    Leave a comment:


  • Buckman86
    replied to The blob!
    Thanks everyone,
    I’ve done flux core for about 2 years now and just starting with mig.
    the wire is silver but it’s .035 solid mig wire from Harbor Freight.
    The machine says positive polarity for solid wire which I have it set in.
    I usually do 1/2 to 1/4 inch stick out....
    See more | Go to post

    Leave a comment:


  • Buckman86
    started a topic The blob!

    The blob!

    Just got a handler 140. I have C25 gas and solid wire. I try to weld and the metal doesn’t melt and the wire just blobs up.
    The gas is at 15 CFH
    I’ve double and triple checked the polarity
    im running speed and voltage based on the chart.
    Im sure I skipped a step somewhere...
    See more | Go to post