I am worried about fertilized water eating the frame up so I added sink drains to control the water. I am sealing the inside quick set cement. I am adding a brace to support the vertical walls.
I cut 45s in the ends of the square tubing to close the ends. ...
Leave a comment:
-
Used a Harbor Freight metal roller to roll 3/16” x 1” flat bar to make the wheels. ...
- 1 like
Leave a comment:
-
Rolling Raised Bed Garden Cart
Built a raised bed gardening cart for a Christmas gift. ...
-
Made some modifications to the design. Added 1/4” x 1” flat bar as vertical supports. Added bolts to secure to the bucket. Got rough with it moving some stumps to test the design. Forks did not bend, bent the bucket...DOUGH! ...