    The lamp frame is from 1-inch square steel tubing. The top of the lamp is 5052-H32 aluminum sheet metal. The flared holes are formed using MITTLER BROS. hand tools. The pendent lamps are from Amazon. The table legs are fabricated from 1/8-inch thick steel flat stock and painted black.

  • #2
    If I had a window to look out folding laundry I'd be a inclined to enjoy the job. Give me lights to boot and I'd be spoiled. Looks good!

    Comment


    • #3
      It looks good.