    Hello. Putting together a new welding table coming along pretty well, I was wondering if anyone had any input..should I put cross bracing on the underside of the table top. Being one inch plate I don' think it will need it but I like over building things just to be sure. Any input is appreciated.

  • #2
    The welding table at work is 1" thick. They never put any cross members under it, and over time it developed some bowing. A new frame was made that has some cross members on it, that the plate is bolted down to. The plate is flatter now, but not as good as it was originally.
    MigMaster 250- Smooth arc with a good touch of softness to it. Good weld puddle wetout. Light spatter producer.
    Ironman 230 - Soft arc with a touch of agressiveness to it. Very good weld puddle wet out. Light spatter producer.


    PM 180C



    HH 125 EZ - impressive little fluxcore only unit

    Comment


    • #3
      Just flip it over once a year and you won't have any issues.