    Do you ever encounter a 15 minute jobs that turn into a three hour job?

    My wife asked me to install a pole for the bird feeder that she purchased. It didn't sound like a welding job but the pole was so short, that she couldn't see the birds at the feeder, which is the whole point of having a bird feeder. I spliced the shaft and then I decided to move the cross brace up so the there would be 16 inches in the ground instead of just 10 inches. I settled on 16 inches because I had underground electrical conduit at 18 inches and I didn't want to hit it.

    1. Removing zinc plating with hydrochloric acid (or Muriatic acid from Home Depot)

    Click image for larger version

Name:	1. Removing zinc plating.jpg
Views:	22
Size:	49.8 KB
ID:	702735

    2. Zinc plating removed (to avoid poisonous fumes when welding)

    Click image for larger version

Name:	2. Zinc plating removed.jpg
Views:	22
Size:	104.0 KB
ID:	702736

    3. Chamfering shaft (to get full penetration)

    Click image for larger version

Name:	3. Chamfering shaft.jpg
Views:	22
Size:	51.7 KB
ID:	702737

    4. Cutting Shaft

    Click image for larger version

Name:	4. Cutting Shaft.jpg
Views:	22
Size:	69.8 KB
ID:	702738

    5. Aligning shaft

    Click image for larger version

Name:	5. Aligning shaft.jpg
Views:	22
Size:	89.8 KB
ID:	702739
    sigpic
    Miller Thunderbolt
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Lincoln LE 31 MP
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport

  • #2
    6. Tack TIG welding shaft (because I have better control of the puddle)

    Click image for larger version

Name:	6. Tack welding shaft.jpg
Views:	22
Size:	76.9 KB
ID:	702741

    7. Shaft TIG welded

    Click image for larger version

Name:	7. Shaft welded.jpg
Views:	21
Size:	90.4 KB
ID:	702742

    8. Cross Brace MIG weld 1 (because it is faster)

    Click image for larger version

Name:	8. Cross Brace weld 1.jpg
Views:	21
Size:	97.3 KB
ID:	702743

    9. Cross brace MIG weld 2

    Click image for larger version

Name:	9. Cross brace weld 2.jpg
Views:	21
Size:	72.7 KB
ID:	702744

    When I went to install the squirrel shield I noticed that the bracket that came with the squirrel shield was too large to fit on the pole. You might think if you purchased both at the same store at the same time that they would fit, but you would be wrong. To solve the problem I machined a Black Delrin plastic spacer to take up the gap. The new spacer does look like it belongs with the bracket.

    10. Boring and cutting off spacer

    Click image for larger version

Name:	10. Boring spacer.jpg
Views:	21
Size:	65.8 KB
ID:	702745
    sigpic
    Miller Thunderbolt
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Lincoln LE 31 MP
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport

    Comment


    • #3
      11 Splitting spacer

      Click image for larger version

Name:	11 Splitting spacer.jpg
Views:	21
Size:	72.3 KB
ID:	702747

      12. Split spacer in place

      Click image for larger version

Name:	12. Split spacer in place.jpg
Views:	21
Size:	40.2 KB
ID:	702748

      13. Squirrel shield installed

      Click image for larger version

Name:	13. Squirrel shield installed.jpg
Views:	21
Size:	61.7 KB
ID:	702749

      14. Bird feeder installed

      Click image for larger version

Name:	14. Bird feeder installed.jpg
Views:	22
Size:	87.4 KB
ID:	702751

      You can see my garage in the background. The part that sticks out in the rear of the picture is my new addition that I have been working on for the past year. The status is that I am almost finished with installing the insulation.
      Attached Files
      sigpic
      Miller Thunderbolt
      Smith Oxyacetylene Torch
      Miller Dynasty 200DX
      Lincoln SP-250 MIG Welder
      Lincoln LE 31 MP
      Clausing/Coldchester 15" Lathe
      16" DuAll Saw
      15" Drill Press
      7" x 9" Swivel Head Horizontal Band Saw
      20 Ton Arbor Press
      Bridgeport

      Comment


      • #4
        Nice Honey Do project Don, you should now be able to throw a hint to the wife of some other new tool you would like to have that would make projects easier.

        Comment


        • #5
          Oooh, that would have been the perfect project for a friction welder!

          Comment


          • #6
            Don I am going to have to file away the pictures of your project for safe keeping for using at just the right time. I saw over on W.W. that you have 8 welders and my other half gives me **** for having 4, and is always mentioning to me and others that I have 4 welders. If I save away the pictures of your project when the wife comes to me wanting a project done I can say if I had the welder collection Don has I could fix you up with a bird feeder like Don made for his wife!

            Comment


            • #7
              Don you remind me of someone I loved watching in the 1990's. Tim the Tool Man Taylor. That's priceless!

              Comment

              Working...
              X