Dave, your welding table in the background looks a little like the one I have right now, except I used a truck wheel for the base and used 3" pipe for the upright on mine. I think my welding table is 24" in diam. How do you like your tubing bender? Does it work pretty good?
Comment
-
Oxy Acetylene Hand truck
gnewby
Mine is also 24" dia. It's 3/8" thick.
The bender you are seeing is not for tubing. It's for bar or round. I find myself just heatng and using a vise for most bending. If you heat and use the bender you can do some real damage. I do have a hydraulic tubing bender."Some days you're the dog, some days you're the fire hydrant"