  • Candle Holder

    First project, little candle holder I made out of scrap.
    When in doubt hit the accelerator, it may not be the right thing to do, but it will sure end the suspense.

  • #2
    Very nice. Did you make the drip trays or buy them from somewhere?

    Darren
    Darren

    Comment


    • #3
      drip trays

      I bought the candle pans from Metalcraft. Very speedy service and excellent to deal with. They have a large array of sizes and many stampings to choose from. You can check them out at WWW.Metalcraftusa.com
      I am thinking of placing a order for metal through them for my first order since the prices seem pretty fair to me. Then once I know what I am looking for I can buy local at a Steel Mart.
      Last edited by Hobweld; 12-15-2003, 02:31 PM.
      When in doubt hit the accelerator, it may not be the right thing to do, but it will sure end the suspense.

      Comment


      • #4
        Nice Hobweld ! What did you use to make the scrolls, and what size flat bar did you use?
        Jim
        Lincoln AC Buzz Box
        HH 175

        Comment


        • #5
          Originally posted by Jim314
          Nice Hobweld ! What did you use to make the scrolls, and what size flat bar did you use?

          Jim314
          I have the Harbor Freight bender with the scrolling attachment. The flat bar is 1x3/16 that I salvaged from the trash bin.
          When in doubt hit the accelerator, it may not be the right thing to do, but it will sure end the suspense.

          Comment


          • #6
            great looking candle holder! Just wait till ya get your 36131 and really go nuts! I recommend the 16 ga candle dishes from metal craft. Their 22 ga stuff is way too thin. I like to use 1/8" flat instead of 3/16". It is easier to bend.
            Art is dangerous!