    I'm what you would call a complete welding newbie. I've been practicing running beads on old lawnmower blades and finally decided it was time to actually build something. I know it ain't much compared to the projects I've seen posted here, but it's mine and my LOML likes it, so that welder has been justified. I've been lurking for awhile and have learned quite a bit from the forum already.
    Hope the pic works.
    Jim
    Lincoln AC Buzz Box
    HH 175

  • #2
    I like it. Got a little artist in ya doncha.
    John

    Comment


    • #3
      jim ,cool
      no one get's out of here alive.

      Comment


      • #4
        eeeeeeeeeehaaaaaaa......do we see a whole fence full of these critters ???
        KenCo " Uccahay "

        Comment


        • #5
          Looks good, Jim...breaks up that plain wall....can ya do a dog next? Is it rebar?

          Comment


          • #6
            Bender - Thanks, no she drew the pattern, I just followed it.
            mozark6 - thanks.
            KenCo - Yep, she's already been drawing more petroglyphs, so I get to weld some more
            RockyD - thanks, I'll ask about the dog. Yep it's rebar
            Jim
            Lincoln AC Buzz Box
            HH 175

            Comment


            • #7
              looks good Jim ! nice looking fence too

              - jack

              Comment


              • #8
                Thanks Jack, took longer than the welding project.
                Jim
                Lincoln AC Buzz Box
                HH 175

                Comment


                • #9
                  Thanks DL !
                  Jim
                  Lincoln AC Buzz Box
                  HH 175

                  Comment


                  • #10
                    JIM what size rebar? heat with a torch?
                    no one get's out of here alive.

                    Comment


                    • #11
                      Thanks guys. It's 3/8" rebar. I did it with my spanking new Lincoln AC buzzbox. 1/8" 6011 sticks.
                      Last edited by Jim314; 10-03-2003, 06:39 PM.
                      Jim
                      Lincoln AC Buzz Box
                      HH 175

                      Comment


                      • #12
                        Man, it looks real good.
                        Those hinges look very sturdy!
                        Challenger 172
                        Thermal Arc 185TSW

                        Comment


                        • #13
                          Yeah their sturdy. I prefer that things don't start sagging when they get older
                          Jim
                          Lincoln AC Buzz Box
                          HH 175

                          Comment


                          • #14
                            Really cool, they do a lot of those from plate with a plasma cutter here in NM, and welcome to the board...
                            Regards, George

                            Hobart Handler 210 w/DP3035 - Great 240V small Mig
                            Hobart Handler 140 - Great 120V Mig
                            Hobart Handler EZ125 - IMO the best 120V Flux Core only machine

                            Miller Dynasty 200DX with cooler of my design, works for me
                            Miller Spectrum 375 - Nice Cutter

                            Comment


                            • #15
                              Thanks George.
                              Jim
                              Lincoln AC Buzz Box
                              HH 175

                              Comment

                              Working...
                              X