Not sure if you all rember me talking about making a 3-point backhoe for my little tractor. Well if you do here is a few pic. I will WORK on getting a better camara and learn to take better shots! LOL
OMS
OMS
HH175
Red Tomstone W/ HF for TIG
Old Miller Engine Driven 225 Amp AC Stick Welder
Smith O/A X 2
Harris O/A
BridgePort
MSC cut off BandSaw 6X12"
And more!
Shop Mechanic for Brinks Coin
Its almost done. Needs bucket teeth and out riggers.
OMS
HH175
Red Tomstone W/ HF for TIG
Old Miller Engine Driven 225 Amp AC Stick Welder
Smith O/A X 2
Harris O/A
BridgePort
MSC cut off BandSaw 6X12"
And more!
Shop Mechanic for Brinks Coin
OMS.......... AND WHAT KIND OF TRACTOR DOES THIS GO ON AND HOW DOES THE HYDRAULIC PUMP HANDLE THE EXTRA LOAD.... ALSO I WOULD LIKE TO KNOW THE PRESSURE REQUIRED FOR THE CYLINDERS............... MAN AIN'T I ASKING A LOT OF QUESTIONS....LET US KNOW HOW IT WORKS...............WHAT SIZE BUCKET TEETH......... I THINK ALL I HAVE ARE JOHN DEERE AND I KNOW THEY ARE TO LARGE..............ROCK...... [email protected]
OMS - Nice job Would it fit my little Kabota 8200? Some times my case back hoe is a little too big and awkword getting into areas on the mountain. As for teeth, I made my ripper teeth out of 5" x 8" steel bar stock welded them on to the ripper shank which I also fabricated and then hardfaced them. Did the same with the bucket on the Kabota only they were 3" L x 1.5" H x .75" W. Spaced 3" apart on the bucket and welded them in place, also hardfaced them. They have been through a lot of hard use for about a year and still havn't had any problems. I could post some pictures of them if you are interested.
Harold
Craftsman Colormatic AC
Victor Journyman Setup
Syncrowave 180 SD
MM210 With Spoolgun
Dynasty 200 DX
Spectrum 625 Plasma Cutter
Miller HD Tape Measure
I have a PTO pump to drive the backhoe. I could have ran it off the tractor but being a hydo drive With a frontloader I thought the pump was already working full time.
I am running 2000 PSI on the system. I think it will handle 2500 MAX.
AS for the teeth. I picked up some 1 1/2 by 2 inch bar stock that I think I can turn in two a few good teeth.
OMS
OMS
HH175
Red Tomstone W/ HF for TIG
Old Miller Engine Driven 225 Amp AC Stick Welder
Smith O/A X 2
Harris O/A
BridgePort
MSC cut off BandSaw 6X12"
And more!
Shop Mechanic for Brinks Coin
It should fit. I put mine on a Kubota B1750. Just have to watch to smaller ones. Like mine. I had to make a SubFrame for the backhoe. The top links will NOT stop the unit for pushing up. SO I made a tie in about half way up the tractors frame. Keeps it from going up. Just have to keep a eye on how far you lift your hitch. Don't whant it to keep trying to lift and burn out a pump.
OMS
OMS
HH175
Red Tomstone W/ HF for TIG
Old Miller Engine Driven 225 Amp AC Stick Welder
Smith O/A X 2
Harris O/A
BridgePort
MSC cut off BandSaw 6X12"
And more!
Shop Mechanic for Brinks Coin
Comment