Announcement

Collapse
No announcement yet.

rod type

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • rod type

    does anybody have any infor mation on E7411 rods?
    uses? manufacturers? etc.
    just found some laying around here at school and no one seems to know anything about them.

  • #2
    I would like to see that electrode. It is not a current AWS designation that I am aware of. Is it smudged and barely legible? If possible can you post a picture of it??
    Respectfully,
    Mike Sherman
    Shermans Welding

    Comment


    • #3
      i don't have any more of them there were only two half burned rods. And i used them in order to see how they burned. I can tell you that they said 7411 on them, and the coating was green and that the beads were like butter.

      Nicest beads i have everseen.

      out of any process

      Comment

      Working...
      X