    Spoolmatics

    Thanks for that confirmation!

    Happy New Year!

    Leave a comment:


  • Hobart Expert
    replied
    Hello Kevin,
    The Spoolmatic 15A is the same as the Spoolmatic 30A other than the length of the cables. Happy Holidays and Happy welding.

    Best Regards,
    Kevin Schuh

    Leave a comment:


  • KMcE
    started a topic Spoolmatic 15A vs 30A

    Spoolmatic 15A vs 30A

    Hello,

    Could someone confirm for me that the only difference between the spoolmatic 15A and the 30A is the length of the cable? It appears that they are 15 ft and 30 ft respectively.

    Thanks
    Kevin