  • Hobart Expert Rock
    Guest replied
    SKYBOSS..........WELL WHAT DID YOU GET............?,,,,,,,,,,,, ROCK
    [email protected]

    Leave a comment:


  • Dan
    replied
    Originally posted by BillC
    The Miller Syncrowave 180SD is the best bang for your buck. I am not sure, but I suspect 1/8" aluminum is probably the limit for this size machine...
    Bill,
    With a good preheat you should be able to weld 3/16" aluminum with your new toy (Syncrowave 180) that your going to be getting.

    Leave a comment:


  • BillC
    replied
    The Miller Syncrowave 180SD is the best bang for your buck. I am not sure, but I suspect 1/8" aluminum is probably the limit for this size machine...

    Leave a comment:


  • skyboss
    started a topic Which TIG?

    Which TIG?

    If I want to be able to weld aluminum and TIG is the only way to go, then what is the most economical brand and model? Keep in mind I am the furthest thing from a professional. Just some hobby projects at home, but I do have 220 VAC service in the garage.