I have tried .030" and .035" steel, .030" stainless, and .030" aluminum. I have since bought the 3/64" rollers/tips to try 3/64" aluminum, but I haven't had the chance to try it yet.
As far as the .030" steel, it seemed to run just as well in short arc. I cannot imagine trying to spray with it, though. The .030" SS wire worked quite well too. I normally use .035" SS, but I mistakenly picked up the wrong spool at the store, and didn't noice it until I started having feed problems.
As far as the .030" steel, it seemed to run just as well in short arc. I cannot imagine trying to spray with it, though. The .030" SS wire worked quite well too. I normally use .035" SS, but I mistakenly picked up the wrong spool at the store, and didn't noice it until I started having feed problems.

Comment