    I picked up a 10# spool Hobart HB28 MIG Wire in .035 had not had a chance to use and would like to know how this wire welds compared to others? appreciate the input.

  • #2
    Chuck,I think Hobart put that wire on their ten pounds,because it is a little softer.It is the best wire I have found bar none.I had some feeding problems with radnor on the ten pound spools,and switched to the HB-28 it solved them all.Plus the arc is a little nicer with the Hobart.It is the only solid wire brand in er70-6 I will buy.