    I am not able to register my HH 135 via the web site. Anyone else have the same problem lately and what did you do about it?


    Thanks

    Maxwell

  • #2
    GOODMORNING MAXWELL............. IS NOT A REAL SERIOUS DEAL.... WE ACTUALLY GO BY THE SERIAL NUMBER OR THE BILL OF SALE.......... IF YOU DO NOT HAVE EITHER OF THOSE 2 REQUIREMENTS THEN WE WOULD GO BY THE REGISTRATION....

    AS A LAST RESORT JUST FILL IT OUT AND SEND IT IN.......... I WILL HAVE BRIAN LOOK AT THE SYSTEM AND MAKE SURE IT IS UP TO SPEED............................HANG IN THERE.........ROCK.........
    [email protected]

    Comment


    • #3
      Thanks Rock,

      I have both those items (serial number and sales receipt), I'll send in the information via snail mail.

      I have enjoyed this board and my new welder!

      I tried some aluminum welding the other day, and it went OK.

      I noticed that the HH135 has a narrow range of material thickness when welding AL. Is this the case or is it me? It seems like welding AL lighter than .065 thick I would just blow holes in it. Yet welding aluminum .09-.187 thick was ok. Any thicker and I could not get any penetration.

      I found that when welding alum. you really have to move the gun fast!!

      Found this setup to be the best:

      Wire: 4043
      Heat: 4
      Wire speed: 80
      Gas: 100% Argon
      CFM: 20-30


      Thanks again.