    can you guys give me a little info about this product, other than whats on the website....ie; storage, user feedback? im doing lots of marine repair and this sounds like the perfect consumable for it. thanks

  • #2
    E7018 is a low hydrogen electrode that requires storage in a 250 degree oven. It is generally used on steel .625" and above or hard to weld steel. It is user friendly, but if not stored properly it is a waste of money. What else would you like to know??
    Respectfully,
    Mike Sherman
    Shermans Welding

    Comment


    • #3
      im referring to fabshield 7018 mike, a self-shielding wellding wire. not e7018 electrodes. Im quite familiar with those

      Comment


      • #4
        Hi Gus, I ran a spool of this thru my LN-25 a couple of years back, worked ok.

        What size are you looking at running?

        Bernie

        Comment


        • #5
          who's gus? the site only shows .o68" and up, but I'll have to contact my local supplier about size and availability. I'm hoping for .045 and .062 to fit my liner. Im curious about storage too. thanks for the input bernie.