    I have narrowed my choice to one of these three. I can get similar prices for each. I am new to welding and know very little beyond the basics. I would greatly appreciate your opinions and pros and cons of each. I will be doing mostly light duty projects and am attracted to the portability of the Inverters. Thanks

  • #2
    The Lincoln welds nice,and I haven't seen the others weld,but I like the analog setup of my Thermal prowave 300 better than every other softpad setup of the others.It's way faster and easier to use than all the rest.I am more amazed with this unit then when I bought it three years ago.Its more money but it is coming down.