    I have an old hobart TR-250 HF machine that was working fine. The torch hit the side of the machine and arced out, and now it doesnot tig. The machine just makes a humming noise when you try to weld. Has this ever happened to any one? Or could any one tell me what is wrong with it?

  • #2
    dland,

    When you depress the foot pedal and scratch the electrode will it start an arc?
    Do you get any high frequency to jump from the electrode to the work piece?