There are two new Econo Twin HF power supplies on Ebay for sale. I can't find any info on these on the Miller web page. Does anyone have more info about these? AC? DC? TIG? MIG?
Hi DJD;
The Econo Twin HF was a D/C,A/C welder 150 amps output at 50% duty cycle. The max amps for A/C TIG was 80 amps at 50% duty cycle, and no remote amp control. The primary voltage was single phase and a single voltage. Make sure you find out what the primary voltage is before you buy it. I say this because they made some that was 460 volts only and it would be costly to change them over to run off 230 volts. The manual should be available from Miller Electric MFG.