    What size all around flux core wire do you guys reccomend, what brand and what type. Also the same for solid wire. Thanks in advance.

    Bob Post
    Bob Post

  • #2
    wire size

    for your HH175 I would recommend .035 solid core. I have used several brands. The Hobart Weld-it brand seems to be readily available. I have not done any flux core welding so I will leave that call to someone else

    Comment


    • #3
      I have had great results with .035 flux core. The best I have run goes by the trade name "Blue Demon"...The worst, "Inweld"
      Arbo & Thor (The Junkyard Dog)
      The Next Loud Noise You Hear Is Me!

      Comment


      • #4
        Hey Arbo

        Do you have any more info on that "blue demon" wire? I did a web search and could not come up with anything. Always willing to try what works for someone else.

        Thanks for any help.
        bitternut

        Comment


        • #5
          www.welding-direct.com sells "Blue Demon" wire. The 2lb spools of ER308L stainless, ER70S6 mild steel and 1lb spool of ER5356 aluminum, I have ordered from them have been "Blue Demon" brand. The 10 lb ER70S6 has been "HTP America Inc." brand. I've not had any problems ordering from them. Only problem is I think they still have a $50.00 minimum order.
          linngl
          Junior Member
          Last edited by linngl; 01-30-2003, 10:38 AM.

          Comment


          • #6
            You can always pad the order by picking up some more tips, nozzles, autodark helmut, sd180, etc.

            Don't let the woman find out though!
            It's not an optical illusion...it just looks like one

            Comment


            • #7
              AL T......... MUM IS THE WORD, OF COURSE IF THEY HAVE MUTUAL CONTROL OVER CHECK BOOK............. THE WORD WILL GET OUT.......YOUR CALL.........................................ROCK
              [email protected]

              Comment

              Working...
              X