    Guest
    Guest

  • Hobart Expert Rock
    Guest replied
    AL T......... MUM IS THE WORD, OF COURSE IF THEY HAVE MUTUAL CONTROL OVER CHECK BOOK............. THE WORD WILL GET OUT.......YOUR CALL.........................................ROCK
    [email protected]

    Leave a comment:

  • Al T.
    Senior Member

  • Al T.
    replied
    You can always pad the order by picking up some more tips, nozzles, autodark helmut, sd180, etc.

    Don't let the woman find out though!

    Leave a comment:

  • linngl
    Junior Member

  • linngl
    replied
    www.welding-direct.com sells "Blue Demon" wire. The 2lb spools of ER308L stainless, ER70S6 mild steel and 1lb spool of ER5356 aluminum, I have ordered from them have been "Blue Demon" brand. The 10 lb ER70S6 has been "HTP America Inc." brand. I've not had any problems ordering from them. Only problem is I think they still have a $50.00 minimum order.
    linngl
    Junior Member
    Last edited by linngl; 01-30-2003, 10:38 AM.

    Leave a comment:

  • bitternut
    Senior Member

  • bitternut
    replied
    Hey Arbo

    Do you have any more info on that "blue demon" wire? I did a web search and could not come up with anything. Always willing to try what works for someone else.

    Thanks for any help.

    Leave a comment:

  • Arbo
    Senior Member

  • Arbo
    replied
    I have had great results with .035 flux core. The best I have run goes by the trade name "Blue Demon"...The worst, "Inweld"

    Leave a comment:

  • cope
    Senior Member

  • cope
    replied
    wire size

    for your HH175 I would recommend .035 solid core. I have used several brands. The Hobart Weld-it brand seems to be readily available. I have not done any flux core welding so I will leave that call to someone else

    Leave a comment:

  • Bob Post
    Junior Member

  • Bob Post
    started a topic Hh175

    Hh175

    What size all around flux core wire do you guys reccomend, what brand and what type. Also the same for solid wire. Thanks in advance.