  • Mowjunk
    replied
    Nope, you need pure argon.......

    You're ahead of the game with the spool gun, though..

    Leave a comment:


  • Dave
    started a topic Aluminum

    Aluminum

    I have a miller 210 w/spoolgun. thinking about welding aluminum. Can I weld aluminum with 75/25argon/co2 gas?