is it pretty? nope
does it hold water? Yep
How many did I go through? didnt waste ANY cans
one try.
Welder: Dynasty 200 DX
Setup: 20 amps, 40 balance, 80 on the frequency, foot pedal, 3/32s 2% thoriated tungsten! its all I had, gotta make due at midnight on friday right? 1/16th 4043 rod, all I had as well.
Total time 1.5 hours.
no holes, and If I have time, Ill TRY to get the right tungsten and rod setup, and go to town
Beer can Pic here!
Louis
does it hold water? Yep

How many did I go through? didnt waste ANY cans

Welder: Dynasty 200 DX
Setup: 20 amps, 40 balance, 80 on the frequency, foot pedal, 3/32s 2% thoriated tungsten! its all I had, gotta make due at midnight on friday right? 1/16th 4043 rod, all I had as well.
Total time 1.5 hours.
no holes, and If I have time, Ill TRY to get the right tungsten and rod setup, and go to town

Beer can Pic here!
Louis
Comment