  • Hobart Expert Dave
    replied
    No it is not. The 175 will only do 1/4" Steel in a single pass. For 1/2" you will need to go with the 250 machine.
    Thanks
    Dave Evans

    Leave a comment:


  • Hobart Expert Rock
    Guest replied
    WJONES43...............WELL ABSOLUTELY NOT..............THE ONLY WAY TO DO 1/2 INCH IS TO "V" IT OUT AND DO SEVERAL PASSES OVER THE ROOT............AMOUNT OF PASSES DEPENDS ON THE WIDTH OF THE "V".............THIS IS STRAIGHT FROM THE HORSES MOUTH...........SORRY.............. NO CAN DO...............ROCK[email protected]

    Leave a comment:


  • wjones43
    started a topic Mm175

    Mm175

    Novice welder here and am getting some conflicting advice about the MM175 mig welder. Is the MM 175 mig welder capable of welding 1/2" steel in one pass ?