Novice welder here and am getting some conflicting advice about the MM175 mig welder. Is the MM 175 mig welder capable of welding 1/2" steel in one pass ?
Announcement
Collapse
No announcement yet.
Mm175
Collapse
X
-
WJONES43...............WELL ABSOLUTELY NOT..............THE ONLY WAY TO DO 1/2 INCH IS TO "V" IT OUT AND DO SEVERAL PASSES OVER THE ROOT............AMOUNT OF PASSES DEPENDS ON THE WIDTH OF THE "V".............THIS IS STRAIGHT FROM THE HORSES MOUTH...........SORRY..............NO CAN DO...............ROCK[email protected]