I would like to try .023 wire and c25 in place of the flux cored wire I have been using on my Handler 135 when welding thin metal.
Do I need to change the liner in the feed hose? What size tip should I use?
TIA,
WarHammer
Do I need to change the liner in the feed hose? What size tip should I use?
TIA,
WarHammer