is it possible to weld stainless steel with an arc welder? if so, there a special electrod I need to use?
Announcement
Collapse
No announcement yet.
ss arc welding?
Collapse
X
-
Yes, stainless is arc welded by all three processes. Stick, Mig and Tig. You need to match the rod with the type being welded and there are several types.
-
Originally posted by streetslide
also, got the number/code of the rod used to weld 304 or 316 ss?MigMaster 250- Smooth arc with a good touch of softness to it. Good weld puddle wetout. Light spatter producer.
Ironman 230 - Soft arc with a touch of agressiveness to it. Very good weld puddle wet out. Light spatter producer.
PM 180C
HH 125 EZ - impressive little fluxcore only unit
Comment
-
Originally posted by streetslide
also, got the number/code of the rod used to weld 304 or 316 ss?
Comment
-
Originally posted by streetslide
an exhaust manifoldMigMaster 250- Smooth arc with a good touch of softness to it. Good weld puddle wetout. Light spatter producer.
Ironman 230 - Soft arc with a touch of agressiveness to it. Very good weld puddle wet out. Light spatter producer.