    Ok guys...I got the three hooks welded to the bucket...used spray transfer...for the most part I think I did ok with the exception where the hook side curved in and I should have weaved a little wider there to make the weld straight...ugh...oh well..
    Short Term Memory GONE!!
    Hobby Weldor/Machinist
    Photobucket Shop Pics

  • #2
    a closer shot
    Short Term Memory GONE!!
    Hobby Weldor/Machinist
    Photobucket Shop Pics

    Comment


    • #3
      I would wrap the ends, Bob and eliminate the possibility of a crack to start.

      Comment


      • #4
        I thought about that Rocky..and didn't do it....But I will now...thanks..