Well, the first one turned out a lot better then I thought it was going to. Here is the second weld.
Announcement
Collapse
No announcement yet.
Tig Fillet 2
Collapse
X
-
Tig Fillet 2
Last edited by Dan; 05-01-2009, 09:13 AM.MigMaster 250- Smooth arc with a good touch of softness to it. Good weld puddle wetout. Light spatter producer.
Ironman 230 - Soft arc with a touch of agressiveness to it. Very good weld puddle wet out. Light spatter producer.
PM 180C