    i am trying to weld the 2 tubes together using ARKSEN mig 100 welder flux core, but failed miserably.
    i did brush cleaned the galvanized area of the 2 steel tubes.
    can somebody help me please?
    (1) is my amp too low?
    (2) is my volt too low?
    Click image for larger version  Name:	75AA6D92-A480-4313-97B7-19BEE91F00D4.jpeg Views:	1 Size:	433.6 KB ID:	708611
    Last edited by W18; 03-21-2020, 09:48 PM.

  • #2
    Here is the ARKSEN mig 100 welder i am usingClick image for larger version

Name:	23C3CD15-AFC5-46E1-9F1B-C3B5E2952296.jpeg
Views:	30
Size:	404.4 KB
ID:	708613

    Comment


    • #3
      First off galvanized if difficult to weld to ... Second there is a issue of inhaling fume from welding galvanizing, look uo "metal fume fever"....

      https://en.wikipedia.org/wiki/Metal_fume_fever

      As for you actual problem it appears almost everything that can be wrong is wrong. I know, no help but....

      You may find your solution here....It's a really good video that defines most common problems and gives solutions...

      https://www.youtube.com/watch?v=Xod-ByrxHg4