    Hello all !, I have a problem with my 125 , i was welding some small pipe and after about 5 min. it quit welding ! the fan works and the push button in the back is in. what could be the problem ? I opened the case to check for anything burnt or blown ,but i found nothing. Any help would be appreciated.

    Thanks Henry

  • #2
    Did your machine ever reset? Sounded like a thermal overload.

    Keith

    Comment


    • #3
      125

      thanks for the resonse ,No it has never reset ,for almst 4 years this the first problem that i had .

      Thanks

      Comment


      • #4
        Does the unit click inside when the trigger is depressed?

        Keith

        Comment


        • #5
          Thank you for sharing your problem!
          I thing there is need to refresh your machine or check its speed then repair, According to me there is just machine renewal problem. Thanks...