    The kid's want to make chimes out of metal. I was going to go to home depot what would be the best metal to buy for a good sounding chime? Thanks for any and all help....

  • #2
    I've had good luck with electrical EMT tubing. Copper is also very good. Serach the web for all the different tunings.
    "Good Enough Never Is"

    Comment


    • #3
      Do a search on making windchimes and you will find more information than you want. A big factor will be how big do you want them to be. I had good luck making a set that was pretty large out of steel tubing, and sounds great. A couple pretty good sites are:

      http://www.geocities.com/teeley2/tuning.html
      http://home.fuse.net/engineering/Chimes.htm
      http://mysite.verizon.net/cllsj/windchimes/home.htm

      Good Luck