  • piekar
    replied
    http://parts.digikey.com/1/parts/100...20-2n6388.html

    is this what i need, the link in the other post didn't work?

    Leave a comment:


  • Hobart Expert Keith
    replied
    The board will need to be replaced or repaired. When the WFS goes to max it is usually Q1 on the board that needs replaced if repairing the board.

    Keith

    Leave a comment:


  • mrandrei
    replied
    Does it have a reset button? If so, it has gone bad, if not there is a fuse or something inside.

    Leave a comment:


  • Zrexxer
    replied
    Yes, it's a known issue. See this thread:

    http://www.hobartwelders.com/weldtal...ad.php?t=31889

    Leave a comment:


  • piekar
    started a topic wire speed control issue on handler 135

    wire speed control issue on handler 135

    i have a handler 135 and the wire speed is stuck on 100. it doesn't change when you turn the knob. are there any known problems for this? is there any test i can do to find the problem?