Has anyone noticed any difference in their welds using a gas lens opposed to the standard collet body?
I run my argon @ 11cfh regardless of the ceramic on the torch, seems to work. The only advantage I've seen so far is my tungsten can stick out a little farther.
This is done with a Multi- Handler 200. Specs are 14 ga. 73 amps, 2% ceriated 1/16 tungsten, 11 cfh argon.
I run my argon @ 11cfh regardless of the ceramic on the torch, seems to work. The only advantage I've seen so far is my tungsten can stick out a little farther.
This is done with a Multi- Handler 200. Specs are 14 ga. 73 amps, 2% ceriated 1/16 tungsten, 11 cfh argon.