    I have a old Hobart porta-flex welder looks like it is 375 or maybe 400 amp unit and it came with a external wire feed for mig welding it also came with a foot pedal and in another box there was a Century High frequency are stabilizer box with this welder and this box can I tig weld aluminum ? I am not sure if this machine is a AC/DC or dc only

  • #2
    The Porta Flex is a DC only machine. It will only TIG weld steel and stainless.