  • EZ-Tig 165i

    Looking at getting the EZ-Tig 165i, but wondering if this will weld silcone bronze? Metal thickness would be 1/4” max. This is for welding small bronze sculptures back together after casting.

  • #2
    It will.... I have done it with an older Miller Syncrowave 180 with no problem. I had better looking beads using AC but DC will work. Remember that the joints will not be as strong as welding. You will actually be brazing more so than welding.

    Good luck with it! And welcome to the forum.

    Mow

    Comment


    • #3
      Great, thanks so much Mow