Help... I am ate up with stupid....

Collapse
X
  • Filter
  • Time
  • Show
Clear All
new posts

  • Help... I am ate up with stupid....

    I just bought a hobart 250 tigwave, and it weld alum. great. I havn't tigged steel in years, so i figured i would try it. Dc- continious off, sharpend my red tungsten.... What the **** am I doing wrong? It won't weld steel for anything. I know I am am doing something stupid wrong here, please help!!!

  • #2
    Are you on DCEN (Electrode negative)?

    Or has your rectier bridge fried?

    vg
    sigpicViceGrip
    Negative people have a problem for every solution

    Comment


    • #3
      I got it.. Just didn't have the remote switch in the right place. I knew it was all my stupid!!!! Thanks for the help!!