    I made the mistake of welding a 2' bead on one side of a 5' square tubing. As you can guess it got distorted. What is the best process to straighten?

    Should I heat it up with a torch?
    Should I weld some beads on the opposite side to see if will bend towards the new weld?
    If anyone could help, I would greatly appreciate it!
    Plez walk me thru step by step.
    Thnk u

  • #2
    More information! (structure, material thickness tools available purpose....????).

    Comment


    • #3
      x2!

      Can you upload some pics? different angles, and of the weld. We'll try to help ya out
      If you don't want an honest answer, don't ask!

      MM 130
      MM 210
      MM 251
      Spectrum 625
      Spoolmatic 200 & 30A
      Synchrowave 180 SD
      Miller BWE x2/Canadian
      Digital elite 'Lucky's speed shop'
      Digital elite 'plain old black' with a sticker paint job
      Henrob/Victor O/A setup

      Comment


      • #4
        Pics are always best.
        Walker
        Chief slag chipper & floor sweeper
        Ironwood Artistic

        Comment

        Working...
        X