    I just got this unit from a friend. He had no idea what he had or how to use it. So today I set it up. He had no manual, no 220 plug. ( I ordered one ) and no consumables. So this is new to me. The torch looks like the tip is called a drag tip and does not need the wire clip. Is that correct ? Also what should I buy for spare consumables ? I gave it a test run today looks like a great machine to have out in my shop. Thanks. Mike

  • #2
    Welcome aboard....

    If you have not found it already, here is manual....

    https://www.hobartwelders.com/files/...72181C_HOB.pdf

    Dale