Howdy!

I have run into a problem that when I start to cut, the arc and air cycle on and off at about twice a second. I refreshed the torch consumables with no luck. Trouble shooting say try to speed up the cut and this will keep the torch lit but I have go too fast to do so which is too fast to cut. this machine has worked flawless for many years at any speed. Need help.

Thanks,
Tom