    Can argon or CO2 be used in a plasma cutter insted of compressed air in a plasma cutter?
    Old Airco 180 amp A.C.

  • #2
    No. But Nitrogen usually can.
    Trailblazer 302 * Millermatic 212 * Syncrowave 180SD * X-Treme 12VS Feeder * Spoolmate 3035
    Thermal Dynamics Cutmaster 52 Plasma * Lincoln 175 MIG

    Victor Superrange II * Victor Journeyman

    Hobart HH 125EZ


    Comment


    • #3
      Using compressed air is relative resent development that makes using plasma cuts affordable for general use. Plasma torches consumables today can withstand compressed air with acceptable life and replacement cost.