    Have an old Hobart 140.
    I've never changed the liner for the hose.
    Is there a reason why it needs to be changed????
    What problem would I have if it's bad?????

  • #2
    Not an expert, but if it's feeding wire and welding OK, just run it. Some suggest blowing the dust particles out of the liner occasionally.
    Miller Challenger 172
    Hobart AC/DC Stickmate
    Older Sears AC stick machine

    Comment


    • #3
      If it doesn't get kinked, most people with a machine that size will never change the liner.

      Comment


      • #4
        No problems at all.
        No kinks.
        Feeds well.
        I guess I'll just leave it alone.