    Converting a Hobart 210 MVP to .023 wire

    So I went to Tractor Supply today to buy a roller and tips for .023 wire. They did not have them and they said they do not carry the rollers only the tips. My understanding is you need a .023 roller for the Hobart 210 MVP welder. Am I wrong? So what do I need to run .023 wire?

  • Hobart Expert Keith
    replied
    The 261157 is currently the standard roller used on the 210MVP. If the unit you have is older then it will not have the tri-groove roller and you will need it to push the .023 wire. The TSC may not carry it but they can order it at the parts counter. Or go http://www.hobartweldshop.com/search...h_query=261157 to order it.

    Leave a comment:


  • Rangerhgm
    replied
    The Drive Roll that came with my 210MVP handles .024 V Groove .030−.035 V Groove (solid wire) and .030-.035 VK Groove (flux core)

    Leave a comment:


  • jwd
    replied
    Originally posted by Dale M. View Post
    Umm...... Parts manual for 210MPV only shows .030-.035 roller for that machine..

    However this may work, seems to be new "universal" roller...

    https://www.hobartwelders.com/consum...ve-roll-261157

    Hope tech support will step in and confirm...

    Dale

    That's what I bought for use with my 210MVP , it works just fine - https://store.cyberweld.com/miqusedrro26.html
    Last edited by jwd; 12-31-2018, 06:42 PM. Reason: spelling

    Leave a comment:


  • oldguyfrom56
    replied
    I know this may sound dumb...but have you tried?

    https://www.hobartwelders.com/files/.../O927L_HOB.pdf

    I'm thinking the "V" groove roller is cut low enough to work? Yup, that simple. Check it and see.

    Leave a comment:


  • Dale M.
    replied
    Umm...... Parts manual for 210MPV only shows .030-.035 roller for that machine..

    However this may work, seems to be new "universal" roller...

    https://www.hobartwelders.com/consum...ve-roll-261157

    Hope tech support will step in and confirm...

    Dale