    Anybody use Stargon ss, and or 309lsi, pretty hot and cannot seem to lower it.
    Weld bead has a blue carbon steel look to it even after brushing.
    Easily see bead drop and crater at end of run backside shows drop.
    running about 280ipm and a power of 3-4 on a low side
    Welder Beta Mig 200