    I dont know if this a dumb question? But can I use Lincoln Flux-Core wire in a Hobart welder?
    Is there any difference in quality?
    Thanks ~Gage~

  • #2
    I don't know why not, I'm using Lincoln L-56 mig wire in my 210. But then I've seen several hundred pounds of it burned at work. Lots of people have a favorite wire, and it's not necessarily Hobart, that they run in their Hobarts.
    Blacksmith
    Stickmate LX AC/DC
    Big cheap (Chinese) Anvil
    Hand cranked coal forge
    Freon bottle propane forge
    HH 210 and bottle of C25

    Comment


    • #3
      just be sure to set your voltage taps correctly for flux core.
      "Good Enough Never Is"