    I have hobart handler 140 that I picked up 2nd hand,it is missing the regulator and hose. It welds fine with the flux core wire but I want to do some sheet metal welding. I have been looking at the Victor cut skil af150-580 part #0781-1103 regulator/flowmeter w/10' hose or the smith H1960-580 regulator w/hose. I plan on using an argon/Co2 mix and was wondering which of these two would be my best choice?
    thank you!!

  • #2
    The Smith is the OEM part. Either one will do the job just fine.