Anyone ever use the 10-11 lb. rolls of wire sold at Harbor freight?Just wondering because the price seems to be very good. thanks
Announcement
Collapse
No announcement yet.
mig wire?
Collapse
X
-
Hey l-h-r,
The HF MIG wire with orange & yellow labels are made in Italy and run very well. I have never had any issue with the Italy made wire and others have found favor with it. DennyComplete weld/mach./fab shop
Mobile unit
"A man's word is his honor...without honor, there is nothing."
"Words are like bullets.... once they leave your muzzle, you cannot get them back."
"I have no hesitation to kill nor reservation to die for the American Flag & the US Constitution."
-
I'll second Yorkie's comments. I've ran a few rolls of the HF ER70S-6 (.035) through my 175+, it works good.Brian
_________________
Hobart Stickmate LX 235AC/160DC
Lincoln SP175 Plus
Hobart (Smith) torch set on Propane
Oxweld C-32 torch (retired, but still ready for service)
Ryobi 14" Chop Saw
HF (Chicago Electric) Metal Cutting Circular Saw
Comment
-
I have run it too with no problems...BobBob Wright, Grandson of Tee Nee Boat Trailer Founder
Metal Master Fab
Salem, Ohio
Birthplace of the Silver & Deming Drill
http://www.ceilingtrains.com/
http://groups.yahoo.com/group/sawking/
http://groups.yahoo.com/group/southbend10k/
Comment
Comment